Water is not simply a foreign substance entering wood from outside or remaining from the tree's water-transport system; it is one of wood's fundamental constituents. A proportion of the water in wood, around 25–30%, is described as chemically bound to the wood fibres.
One criticism of wood is its movement: dimensional change when it becomes wet or when ambient humidity changes. Complaints such as “My window has warped and no longer closes properly” or “It swelled in the rain and will not open” are familiar. However, these problems can be avoided by selecting and drying timber correctly and designing the component properly. All materials move. The text describes wood as not changing dimensions or softening and hardening with heat; its significant movement is associated with water and occurs across the grain rather than along it. This gives designers considerable scope for spanning large distances without elaborate detailing to accommodate day-to-night temperature differences. Twisting during moisture-related dimensional change can be limited by attention to straight grain. Where this is particularly important, quarter-sawn timber may be used.
Moisture content
Wood moisture content is expressed as a percentage of its oven-dry weight. A piece containing equal weights of dry fibre and water therefore has a moisture content of 100%. Green timber may consequently have a moisture content much higher than 100%.
Freshly felled timber retains its principal dimensions until its water content falls to approximately 30% of its dry weight. Below this fibre-saturation point, it shrinks as it dries. Likewise, dry timber swells as its moisture content rises towards approximately 30%; increases above this level do not cause further swelling.
Moisture movement may also cause deflection, buckling and cracking. Although changes in relative humidity affect timber moisture content and movement, rainwater penetration is the main concern for external timber. End-grain surfaces are especially important, as they can absorb water hundreds of times faster than side-grain surfaces. In species with low permeability, water entering the end grain may cause only slight, localised wetting. In more permeable species, including softwoods, moisture can spread rapidly and extensively, readily reaching levels above 100%.
However carefully wood has been dried, subsequent wetting can change its properties and its ability to hold paint, even if it has been treated against decay. Exterior timber in direct contact with water therefore needs microporous coatings that resist liquid-water penetration while allowing water vapour to escape.