TRADITIONAL METHODS OF PROTECTING WOOD

HOME BLOG TRADITIONAL METHODS OF PROTECTING WOOD
TRADITIONAL METHODS OF PROTECTING WOOD

Does wood really need protection? The burial chamber of King Midas, or according to some sources his father, dating from 800 BC remains intact, yet facade cladding installed today can decay within a year. To understand why, this section examines traditional methods of protection and present-day requirements. Traditionally, protection against biological deterioration has rested on two ideas: natural durability and keeping wood dry.

What is natural durability?

One traditional way of extending the life of timber buildings is to choose naturally durable species such as oak and chestnut for structural members or locations at high risk of decay. Heartwood, the inner part of the tree, contains natural substances that protect against wood-destroying organisms. Its durability varies by species.

  • Maple, beech and poplar: less than five years.
  • Pine, fir and spruce: five to ten years.
  • Chestnut, cedar and oak: fifteen to twenty-five years.

These figures refer only to the heartwood's resistance to fungi when in direct contact with soil. The outer sapwood of every species decays readily. The figures also exclude damage from termites, marine borers and other insects.

How can wood be kept dry?

Wood-destroying organisms need oxygen, warmth and water to survive and develop. Keeping timber dry, below 20% moisture content, can therefore control decay to a degree. Coffins made from maple, a non-durable species, have survived in the hot, dry environment of Egyptian pyramids. One reason traditional Turkish houses have wide eaves is to protect timber facades from rain.

Keeping wood dry throughout its service life is difficult. Exterior timber is wetted by rain; indoor timber can be wetted by faulty plumbing, leaking roofs and condensation. Moisture can readily reach levels suitable for decay. Even if the timber itself is kept dry, dry-rot fungi can transport the water they need over long distances, and termites can also cause destruction.

Another approach is to cover the surface with a waterproof layer, or paint it. Wood movement, however, can soon crack the film. Water entering through these cracks wets the timber and, worse, may be unable to evaporate through the coating, creating ideal conditions for fungal growth. Applying filler and highly vapour-resistant paints to external timber is therefore problematic. Exterior wood should not be covered with filler, and breathable wood coatings should be used.

Developments in the building industry

When timber was plentiful and inexpensive, structural sections were much larger than necessary. Mature trees with little sapwood were felled, so sapwood formed only a small part of finished members and contributed little to their structural strength. Today, advances in timber engineering allow precise load calculations and smaller sections. Construction timber also increasingly comes from plantation-grown trees with a high proportion of sapwood, which is non-durable in every species.

The twentieth century introduced new materials and technologies. Unless properly understood and applied, these innovations may create problems rather than solve them.

Condensation

Lifestyles changed during the twentieth century. Indoor plumbing and appliances such as washing machines greatly increased the amount of water vapour produced in homes. Faulty services and burst pipes can also raise the moisture content of structural timber above 20% from time to time.

Roof insulation

Where insulation is incorrectly installed and roof ventilation is inadequate, accidentally wetted roof timbers may decay quickly. Timber that becomes wet and dries promptly does not decay, but insulation that prevents drying can create a serious decay problem.

New surface coatings

The chemical industry has produced paints, varnishes, polyurethanes and epoxies with exceptional properties. Their number and variety can also cause confusion and make product selection difficult. A finish for parquet flooring needs resistance to wear, while an external coating needs flexibility and resistance to sunlight. These developments have pushed traditional preservation methods to their limits and encouraged new protective technologies.

Preservative pretreatment

Wood pretreatment, formerly called impregnation, introduces chemicals into timber to protect it against damaging fungi and insects. It is applied once, before installation, with the aim of ensuring that the material lasts at least as long as the building.

Pretreatment is a specific technology. The chemicals and methods depend on the species, the exposure conditions and the required service life. Some applications require pressure treatment in a dedicated plant; others may need only a simple dipping process. Pretreatment makes wood a dependable modern engineering material with a defined service life. British standards are cited as giving preservative-treated pine joinery a service life of sixty years. The text describes wood as outlasting concrete, steel and plastic.

Wood-preservation technology reached Türkiye in 1915. At the time described here, there were twenty-six plants, eight dedicated solely to joinery and other construction timber, yet less than 1% of timber joinery received pretreatment.

Pretreatment or impregnation?

Türkiye's first treatment plant was established in 1915. At that time, Britain used the expressions “wood preservation” and “timber impregnation plants”. The text notes that “impregnation” was not used in this sense in the United States and had also fallen out of use in Britain, while “preservation” could suggest embalming. It argues that the Turkish term “emprenye” should change for three reasons.

  • “Impregnation” means saturation and does not clearly express the purpose of the treatment.
  • It is sometimes confused with “impermeable”, leading people to think it prevents wood from absorbing water.
  • Expressions such as “impregnating stains” are used, particularly in Central Europe, for penetrating wood coatings and primers also sold in Türkiye.

Some of these coatings contain active ingredients, adding to the confusion. Those ingredients may act only against surface mould and not against the decay fungi that damage the wood structure. Manufacturers sometimes use these products in place of true pretreatment materials, either in good faith or deliberately.

This website provides detailed information about the meaning, importance and application of pretreatment and preservative products. As a guide for consumers, a genuine preservative's technical literature and label should identify the active chemicals and the international standards it meets.

+90 532 789 08 83